Wirebond Workmanship: Sharp Bends or Kinks
Wirebond Workmanship Contents
There shall be no sharp bends or kinks in bonding wires that reduce the wire diameter by greater than 25 percent.

Courtesy Rockwell Collins
Wirebond Workmanship Contents
There shall be no sharp bends or kinks in bonding wires that reduce the wire diameter by greater than 25 percent.
Courtesy Rockwell Collins